Thin Films
Growing films from a few atoms to a few microns thick, where substrate temperature, gas, pressure, geometry and power all shape the result.
Plasma sources
RF plasma deposition runs at the standard 13.56 MHz. Electron cyclotron resonance sources work at about 10⁻⁵ to 10⁻³ Torr with ionisation ratios near 10⁻³ to 10⁻¹, compared with roughly 10⁻⁶ to 10⁻⁴ for RF plasma.
Chemical vapour deposition
Reactor temperature is measured with thermocouples or optical pyrometers. Gas flow is measured with rotameters or, more and more, electronic flow meters that make automation possible. Pressure is held either by changing the inflow at a fixed pumping rate or by throttling the pump.
Hot-wall tube reactors use fully developed laminar flow to deposit polysilicon, silicon dioxide and silicon nitride. Low-temperature reactors at 350–450 °C lay down passivation layers such as silicon nitride over aluminium.
- Reaction chamber
- Power source and matching network
- Gas flow control
- Pressure measurement